DIN EN ISO 5817:2023-07
Welding - Fusion-welded joints in steel, nickel, titanium and their alloys (beam welding excluded) - Quality levels for imperfections (ISO 5817:2023); German version EN ISO 5817:2023
| Fecha edición: |
2023-07-01
En Vigor
|
|---|---|
| Idiomas disponibles: | Inglés, Alemán |
| Resumen: | This standard provides guidance on levels of imperfections in arc-welded joints (beam welding excluded) for all types of steel, nickel, titanium and their alloys. It applys for material thicknesses over 0,5 mm. Levels of imperfections for beam welded joints contains ISO 13919-1. The levels of imperfections are specified in such a way that a broad application in production is possible. The quality levels of imperfections are classified by B, C and D, where B is the quality most difficult to achieve. |
| Keywords: | Acceptance inspection|Alloy steels|Alloys|Arc welding|Butt seams|Defects|Definitions|Design|Evaluation groups|Evaluations|Fillet welds|Fitness for purpose|Fusion welded joints|Fusion welding|Guidelines|Irregularities|Limits (mathematics)|Manufacturing|Nickel|Quality|Quality assurance|Specification (approval)|Steel welding|Steels|Surveillance (approval)|Symbols|Testing|Thickness of the weld seam|Titanium|Unalloyed steels|Welded joints|Welding|Welding engineering|Weldings|Welds |
| ICS: | 25.160.40 - Uniones soldadas y soldaduras |
| CTN: | |
|
Equivalencia Internacional |
Idéntica EN ISO 5817:2023 Idéntica ISO 5817:2023 |
|
Reemplazo Normas |
Reemplaza a DIN EN ISO 5817:2014-06 Reemplaza a DIN EN ISO 5817:2021-08 |