ASTM D2838 - 09
Standard Test Method for Shrink Tension and Orientation Release Stress of Plastic Film and Thin Sheeting
| Aviso: | Las normas ASTM en lectura se visualizan a través del área decliente. Los archivos no se pueden descargar |
|---|---|
| Fecha edición: |
2009-05-01
Anulada
|
| Fecha de anulación: | 2009-05-01 |
| Idiomas disponibles: | Inglés |
| Resumen: | |
| Keywords: | film; orientation release stress; shrink force; shrink tension; thin sheeting; Force; Heating tests--plastics; Heat-shrinkable plastic film/sheeting; Orientation release stress; Plastic sheet and film; Shrinkage--plastics; Shrink force; Stress--plastics; Tensile properties/testing--plastics; Thermoplastics; Thin sheeting |
| Scope: | 1.1 This test method covers the determination of the shrink tension and related characteristics, that is, shrink force and orientation release stress, of heat-shrinkable plastic film and sheeting of less than 1.0 mm (0.04 in.) thickness. Two procedures are described that permit the measurement of shrink forces at predetermined temperatures. They are as follows: 1.1.1 Procedure A is designed to measure the maximum force exerted by a specimen that is totally restrained from shrinking as it is heated rapidly to a specific temperature. 1.1.2 Procedure B is designed to measure the maximum force exerted by a specimen that is permitted to shrink a predetermined amount prior to restraint while being heated rapidly to a specific temperature. 1.2 Orientation release stress can be determined from the data obtained using Procedure A. 1.3 The values stated in SI units are to be regarded as the standard. The values in parentheses are for information only. 1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Note 1—Film has been arbitrarily defined as sheeting having nominal thickness not greater than 0.25 μm (0.010 in.). Note 2—There is no known ISO equivalent to this test method. |
| ICS: | 83.140.10 - Películas y hojas |
| CTN: | D20.19 - D20.19 |
|
Anulaciones Normas |
Anula a D2838-08 |
|
Otras Relaciones |
Es referenciada por D6287-17 Es referenciada por D2673-14R22 Es referenciada por D8065/D8065M - 16(2023) |