Filtrar:
SAE
SAE AMS3901/10
En Vigor
2011-08-09
YARN, ORGANIC FIBER (PARA-ARAMID), HIGH MODULUS OY 390,000 (2690)
Tensile Strength, 16,500,000 (115) Tensile Modulus 1140 Denier, 1.2% Finish
SAE
SAE AMS4165H
En Vigor
2013-12-03
Aluminum Alloy, Extrusions 4.4Cu - 1.5Mg - 0.60Mn (2024-T3511) Solution
Heat Treated, Stress-Relieved by Stretching, and Straightened
SAE
SAE AMS4080H
En Vigor
1968-11-01
ALUMINUM ALLOY TUBING, SEAMLESS, DRAWN 1.0Mg - 0.60Si - 0.30Cu - 0.20Cr (6061-0)
SAE
SAE AMS4349C
En Vigor
1995-04-01
CORE, HONEYCOMB, ALUMINUM ALLOY, CORROSION INHIBITED For Sandwich
Construction 5056,350(177)
SAE
SAE AMS4223B
En Vigor
1995-05-01
ALUMINUM ALLOY CASTINGS 4.5Cu - 0.70Ag - 0.30Mn - 0.25Mg - 0.25Ti
(A201.0-T4) Solution Heat Treated and Naturally Aged
SAE
SAE AMS4179D
En Vigor
2016-09-01
Aluminum Alloy Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7175-T7452)
Solution Heat Treated, Stress Relieved, and Precipitation Heat Treated
SAE
SAE AMS4465A
En Vigor
2015-06-04
Aluminum Alloy, Clad One Side Sheet 0.6Mg - 0.35Si - 0.28Cu (No. 23
Brazing Sheet) As Fabricated
SAE
SAE AMS4442F
En Vigor
2007-01-09
Magnesium Alloy Sand Castings 3.2 Rare Earths - 2.5Zn - 0.70Zr
(EZ33A-T5) Precipitation Heat Treated
SAE
SAE
SAE AMS4323B
En Vigor
2008-05-02
Aluminum Alloy, Hand Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr
(7075-T7452) Solution Heat Treated, Stress Relieved, and Precipitation
Heat Treated
SAE
SAE
SAE AMS4992C
En Vigor
2018-06-03
Casting, Structural Investment, Titanium Alloy 6Al - 4V Hot
Isostatically Pressed
SAE
SAE
SAE
SAE
SAE AMS3798/2B
En Vigor
1999-01-01
Webbing, Low Modulus Aramid 1 (25) Wide, 600 (2669) Breaking Strength
Herringbone Twill
SAE
SAE AMS3670/2B
En Vigor
2006-01-06
Polyamide-Imide Bar, Rod, and Shapes 20 Graphite - 3
Polytetrafluorethylene (PTFE) Filled
SAE
SAE AMS4044F
En Vigor
1983-04-01
ALUMINUM ALLOY SHEET AND PLATE 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-0) Annealed
SAE
SAE