Filtrar:
SAE
SAE
SAE AMS4928B
En Vigor
1965-02-15
TITANIUM ALLOY BARS AND FORGINGS 6Al - 4V Annealed, 120,000 psi Yield
SAE
SAE
SAE
SAE AMS5340D
En Vigor
2011-10-10
Steel, Corrosion Resistant, Investment Castings 14Cr - 4.25Ni - 2.25Mo -
0.25Cb - 3.25Cu Homogenization and Solution Heat Treated
SAE
SAE
SAE AMS3655D
En Vigor
2018-11-20
Tubing, Electrical Insulation Thin Wall, Extruded
Polytetrafluoroethylene (PTFE)
SAE
SAE
SAE AMS4987E
En Vigor
2015-01-15
Titanium Alloy, Forgings 10V - 2Fe - 3AI Consumable Electrode Melted,
Single-Step Solution Heat Treated and Overaged 140 ksi (965 MPa) Tensile Strength
SAE
SAE AMS4907E
En Vigor
1988-04-01
TITANIUM ALLOY SHEET, STRIP, AND PLATE 6.0Al - 4.0V, Extra Low
Interstitial Annealed
SAE
SAE
SAE
SAE AMS3138/2A
En Vigor
1990-07-01
COATING MATERIAL, FLUOROCARBON (FKM) ELASTOMERIC Rain-Erosion and
Thermal-Flash Resistant, White
SAE
SAE AMS4161A
En Vigor
1966-03-01
ALUMINUM ALLOY EXTRUSIONS 1.0Mg - 0.60Si - 0.30Cu - 0.20Cr (6061-T4)
SAE
SAE AMS5442B
En Vigor
2022-08-04
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings
Ni - 18Cr - 2.8Mo - 5.5Cb(Nb) - 0.70Ti - 1.50Al - 10Fe - 9Co - 1W
Consumable Electrode Remelted or Vacuum Induction Melted 1775 °F (968
°C) Solution and Precipitation Heat Treated
SAE
SAE AMS4900S
En Vigor
2023-07-24
Titanium Sheet, Strip, and Plate Commercially Pure Annealed, 55 ksi (379
MPa) Yield Strength
SAE
SAE AMS4242A
En Vigor
1997-09-01
Aluminum Alloy, Castings 4.7Cu - 0.60Ag - 0.35Mn - 0.25Mg - 0.25Ti
(B201.0-T7) Solution Heat Treated and Overaged
SAE
SAE AMS4308B
En Vigor
2017-04-04
Aluminum Alloy, Sheet 8.6Fe - 1.8Si - 1.3V (8009-H112) Powder Metallurgy
Product, Strain Hardened
SAE
SAE