AENOR Logo

Normas SAE

49877 Resultados disponibles

Filtrar:

(40986)
(8891)
SAE

SAE AMS4226B

En Vigor
2017-04-06
Aluminum Alloy Castings, High Strength 5.0Cu - 0.35Mn - 0.18Zr - 0.10V (224.0) Solution and Precipitation Heat Treated (Overaged)
SAE

SAE AMS4434K

En Vigor
1994-04-01
MAGNESIUM ALLOY CASTINGS, SAND 9.OAl - 2.OZn (AZ92-T6) Solution and Precipitation Heat Treated
SAE

SAE AMS4967D

En Vigor
1972-05-15
TITANIUM ALLOY BARS AND FORGINGS 6Al - 4V Annealed, Heat Treatable
SAE

SAE AMS4387D

En Vigor
1994-04-01
MAGNESIUM ALLOY EXTRUSIONS 2.3Zn - 0.62Zr (ZK21A-F) As Extruded
SAE

SAE AMS4930H

En Vigor
2015-01-15
Titanium Alloy Bars, Wire, Forgings, and Rings 6Al - 4V, Extra Low Interstitial Annealed
SAE

SAE AMS4778D

En Vigor
1989-07-01
BRAZING FILLER METAL, NICKEL ALLOY 92Ni - 4.5Si - 3.1B 1800° - 1900°F Solidus-Liquidus Range
SAE

SAE AMS5328A

En Vigor
1973-12-01
STEEL CASTINGS, INVESTMENT 0.80Cr - 1.8Ni - 0.35Mo (0.28 - 0.36C) (SAE 4330 Modified)
SAE

SAE AMS4901B

En Vigor
1955-08-15
TITANIUM SHEET AND STRIP Annealed - 70,000 psi Yield
SAE

SAE AMS4164A

En Vigor
1962-01-01
ALUMINUM ALLOY EXTRUSIONS 4.4Cu - 1.5Mg - 0.6Mn (2024-T3510) Stress-Relief Stretched, Unstraightened
SAE

SAE AMS3798/5C

En Vigor
2015-04-14
Webbing, Low Modulus Aramid 1-23/32 (44) Wide, 3600 (16,014) Breaking Strength Herringbone Twill, Resin Treated
SAE

SAE AMS4414

En Vigor
2019-09-19
Aluminum Alloy, Hand Forgings 7.5Zn - 1.6Cu - 1.5Mg - 0.12Zr (7085-T7452) Solution Heat Treated, Compression Stress-Relieved, and Overaged
SAE

SAE AMS4778H

En Vigor
2006-10-06
Nickel Alloy, Brazing Filler Metal 92Ni - 4.5Si - 3.1B 1800 to 1900 °F Solidus-Liquidus Range
SAE

SAE AMS4124C

En Vigor
1997-04-01
ALUMINUM ALLOY, ROLLED OR COLD FINISHED BARS, RODS, AND WIRE 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T7351) Solution Heat Treated, Stress Relieved by Stretching, and Overaged
SAE

SAE AMS4347C

En Vigor
2007-11-21
Aluminum Alloy Sheet 1.0Mg - 0.8Si - 0.8Cu - 0.5Mn (6013-T4) Solution Heat Treated and Naturally Aged
SAE

SAE AMS4348A

En Vigor
1984-07-01
HONEYCOMB CORE, ALUMINUM ALLOY, CORROSION INHIBITED For Sandwich Construction 5052, 350 (175)
SAE

SAE AMS4173F

En Vigor
2013-04-19
Aluminum Alloy, Extrusions 1.0Mg - 0.60Si - 0.30Cu - 0.20Cr (6061-T6511 or T6510) Solution Heat Treated, Stress Relieved by Stretching, Straightened, and Precipitation Heat Treated
SAE

SAE AMS4427

En Vigor
2000-09-01
Magnesium Alloy Sand Castings 4.0Y - 2.3Nd - 0.7Zr (WE43A - T6) Solution and Precipitation Heat Treated
SAE

SAE AMS5590C

En Vigor
1993-04-01
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SEAMLESS TUBING 52.5Ni - 19Cr - 3.0Mo - 5.1(Cb + Ta) - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1950 °F (1066 °C) Solution Heat Treated
SAE

SAE AMS5622D

En Vigor
2004-12-14
Steel, Corrosion Resistant, Bars, Wire, Forgings, Tubing, and Rings 16Cr - 4.0Ni - 0.30Cb - 4.0Cu Solution Heat Treated, Precipitation Hardenable
SAE

SAE AMS5649J

En Vigor
2024-03-01
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, and Stock for Forgings, 18Cr - 13Ni - 2.1Mo (316FM) Free Machining Solution Heat Treated