Filtrar:
SAE
SAE AMS5343A
En Vigor
1972-11-01
STEEL CASTINGS, INVESTMENT, CORROSION RESISTANT 16Cr - 4.0Ni -3.1Cu
Solution and Precipitation Heat Treated, 150,000 psi (1034 MPa) Tensile Strength
SAE
SAE
SAE AMS5329A
En Vigor
1965-02-01
STEEL CASTINGS, SAND 0.80Cr - 1.8Ni - 0.35Mo (0.28 - 0.36C) (SAE 4330 Modified)
SAE
SAE AMS4770J
En Vigor
1992-04-01
SILVER ALLOY BRAZING FILLER METAL 50Ag - 18Cd - 16.5Zn - 15.5Cu 1160 to
1175 °F (627 to 635 °C) Solidus-Liquidus Range
SAE
SAE AMS4779K
En Vigor
2018-02-06
Nickel Alloy, Brazing Filler Metal 94Ni - 3.5Si - 1.8B 1800 °F (982 °C)
Solidus, 1950 °F (1066 °C) Liquidus
SAE
SAE AMS4385K
En Vigor
2006-10-30
Magnesium Alloy, Sheet and Plate, 3.2Th - 0.70Zr, Cold Rolled and
Partially Annealed
SAE
SAE AMS3822
En Vigor
1994-04-01
CLOTH, TYPE "E" GLASS "B" Stage Epoxy Resin
Impregnated Style 181 - 75DE
SAE
SAE AMS4966R
En Vigor
2017-06-05
Titanium Alloy, Forgings 5Al - 2.5Sn Annealed, 110 ksi (758 MPa) Yield Strength
SAE
SAE AMS4978F
En Vigor
2011-06-23
Titanium Alloy Bars, Wire, Forgings, and Rings 6Al - 6V - 2Sn Annealed
SAE
SAE
SAE
SAE
SAE
SAE AMS4616C
En Vigor
1976-07-01
SILICON BRONZE BARS, FORGINGS, AND TUBING 92Cu - 3.2Si - 2.8Zn - 1.5Fe
SAE
SAE AMS5389B
En Vigor
2011-08-10
ALLOY CASTINGS, SAND, CORROSION AND HEAT RESISTANT 55Ni - 16.5Cr - 17Mo
- 4.5W - 5.8Fe - 0.40V Solution Heat Treated
SAE
SAE AMS3777/9A
En Vigor
1993-01-01
TAPE, NYLON, NONMELTING, REINFORCING 2 (50) Wide, 3000 (13, 345 N)
Breaking Strength
SAE
SAE AMS4447F
En Vigor
2006-06-21
Magnesium Alloy Castings, Sand, 3.3Th - 2.1Zn - 0.75Zr (HZ32A-T5),
Precipitation Heat Treated
SAE
SAE AMS4769F
En Vigor
2009-06-10
Silver Alloy, Brazing Filler Metal 45Ag - 24Cd - 16Zn - 15Cu 1125 to
1145 °F (607 to 618 °C) Solidus-Liquidus Range
SAE
SAE
SAE AMS4259A
En Vigor
2008-11-21
Aluminum Alloy, Sheet 2.4Li - 1.3Cu - 0.95Mg - 0.10Zr (8090-T6) Solution
and Precipitation Heat Treated (Unrecrystallized)