AENOR Logo

Normas SAE

49877 Resultados disponibles

Filtrar:

(40986)
(8891)
SAE

SAE AMS6418D

En Vigor
1972-05-15
STEEL BARS, FORGINGS, TUBING, AND RINGS 1.3Mn - 1.5Si - 0.30Cr - 1.8Ni - 0.40Mo (0.23 - 0.28C)
SAE

SAE AMS5555E

En Vigor
2013-04-09
Nickel and Wire Ribbon 99Ni
SAE

SAE AMS5645J

En Vigor
1976-07-01
STEEL BARS, FORGINGS, TUBING, AND RINGS, CORROSION AND HEAT RESISTANT 18Cr - 10Ni - 0.40Ti (SAE 30321)
SAE

SAE AMS5878A

En Vigor
1996-01-01
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SHEET, STRIP, AND PLATE 59Ni - 22Cr - 2Mo - 14W - 0.35Al - 0.03La Solution Heat Treated
SAE

SAE AMS5744D

En Vigor
2000-09-01
Steel, Corrosion and Heat Resistant, Bars and Forgings 15.5Cr - 4.5Ni - 2.9Mo - 0.10N Heat Treated, 170 ksi (1172 MPa) Tensile Strength
SAE

SAE AMS5844A

En Vigor
1979-07-01
ALLOY BARS, WORK STRENGTHENED, CORROSION RESISTANT 20Cr - 35Ni - 35Co - 10Mo Solution Heat Treated and Cold Drawn
SAE

SAE AMS6354B

En Vigor
1979-07-16
STEEL SHEET, STRIP, AND PLATE 0.75Si - 0.62Cr - 0.20Mo - 0.10Zr (0.10 - 0.17C)
SAE

SAE AMS4017K

En Vigor
2017-11-14
Aluminum Alloy Sheet and Plate 2.5Mg - 0.25Cr (5052-H34) Strain-Hardened, Half-Hard, and Stabilized
SAE

SAE AMS5884E

En Vigor
2022-09-14
Iron-Nickel Alloy, Bars, Forgings, and Rings 42Fe - 37.5Ni - 14Co - 4.8Cb (Nb) - 1.6Ti Solution Heat Treated, Precipitation Hardenable Multiple Melted, High Temperature, Low Expansion
SAE

SAE AMS4109

En Vigor
1995-05-01
ALUMINUM ALLOY HAND FORGINGS 5.6Zn - 2.5Mg - 1.6Cu - 0.24Cr (7175-T736)
SAE

SAE AMS5836A

En Vigor
1995-12-01
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, WELDING WIRE 72Ni - 3.0Mn - 20Cr - 2.5Cb
SAE

SAE AMS5852C

En Vigor
1994-04-01
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, BILLETS AND PREFORMS 55Ni - 15Cr - 17Co - 5.0Mo - 3.5Ti - 4.0Al - 0.0258 Powder Metallurgy Product, Hot Isostatically Pressed
SAE

SAE AMS5663K

En Vigor
2002-11-21
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 52.5Ni - 19Cr - 3.0Mo - 5.1Cb - 0.90Ti - 0.50Al - 18Fe Consumable Electrode or Vacuum Induction Melted 1775 °F (968 °C) Solution and Precipitation Heat Treated
SAE

SAE AMS5734G

En Vigor
1995-05-01
STEEL, CORROSION AND HEAT RESISTANT, BARS, WIRE, FORGINGS, AND TUBING 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted, 1650 °F (899 °C) Solution Heat Treated
SAE

SAE AMS4143B

En Vigor
1984-07-01
ALUMINUM ALLOY FORGINGS 6.3Cu - 0.30Mn - 0.18Zr - 0.10V - 0.06Ti (2219-T6) Solution and Precipitation Heat Treated
SAE

SAE AMS5734F

En Vigor
1989-07-01
STEEL BARS, FORGINGS, AND TUBING, CORROSION AND HEAT RESISTANT 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted, 1650°F (899°C) Solution Heat Treated
SAE

SAE AMS6411F

En Vigor
2006-03-10
Steel Bars, Forgings, and Tubing 0.88Cr - 1.8Ni - 0.42Mo - 0.08V (0.28 - 0.33C) Consumable Electrode Remelted
SAE

SAE AMS4033

En Vigor
1960-06-01
ALUMINUM ALLOY PLATE 4.5Cu - 1.5Mg - 0.6Mn (2024-T351) Stress-Relief Stretched
SAE

SAE AMS4132E

En Vigor
2006-04-24
Aluminum Alloy, Die and Hand Forgings, Rolled Rings, and Forging Stock 2.3Cu - 1.6Mg - 1.1Fe - 1.0Ni - 0.18Si - 0.07Ti (2618-T61) Solution and Precipitation Heat Treated
SAE

SAE AMS5791B

En Vigor
2004-02-10
Cobalt Alloy, Powder, Plasma Spray 56.5Co - 25.5Cr - 10.5Ni - 7.5W