SAE AMS4287C
Aluminum Alloy, Extrusion, 2.7Cu - 1.8Li - 0.7Zn - 0.3Mn - 0.3Mg - 0.08Zr (2099-T83), Solution Heat Treated, Stress Relieved by Stretching 1 to 4% and Aged
| * Secure PDF notice: |
The PDF document of the SAE standards that is downloaded will be locked and cannot be transferred to another computer; it is for a single workstation and a single user. The end user must have the FILE OPEN PLUG-IN security system installed. The document can be printed once. |
|---|---|
| Edition date: |
2025-02-25
In Force
|
| Available languages: | English |
| Summary: | This specification covers an aluminum alloy in the form of extruded bars, rods, and profiles (shapes) produced with nominal thickness up to 3.000 inches (76.20 mm), inclusive, and having a cross-sectional area of 42 square inches (271 cm
2x) maximum and a circumscribing circle diameter (circle size) of 15 inches (38 cm) maximum (see