SAE AMS2759/2E
Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher
| * Secure PDF notice: |
The PDF document of the SAE standards that is downloaded will be locked and cannot be transferred to another computer; it is for a single workstation and a single user. The end user must have the FILE OPEN PLUG-IN security system installed. The document can be printed once. |
|---|---|
| Edition date: |
2009-07-20
In Force
|
| Available languages: | English |
| Summary: | This specification, in conjunction with the general requirements for steel heat treatment covered in AMS2759, establishes the requirements for heat treatment of low-alloy steel parts to minimum ultimate tensile strengths of 220 ksi (1517 MPa) and higher. Parts are defined in AMS2759. |