SAE AMS4640E

In Force
1991-07-01
ALUMINUM BRONZE BARS, RODS, SHAPES, TUBES, AND FORGINGS 81.5Cu - 10.0Al - 4.8Ni - 3.0Fe Annealed
SAE

SAE AMS3894/7A

In Force
1983-04-01
CARBON (GRAPHITE) FIBER TAPE AND SHEET Epoxy Resin Impregnated G 90,000 (620) Tensile, 40,000,000 (275) Modulus, 80 (180)
SAE

SAE AMS4558J

In Force
2022-09-08
Brass, Seamless Tubing 66.5Cu - 31.5Zn - 1.6Pb Drawn Temper (H58)
SAE

SAE AMS4954D

In Force
1984-04-01
TITANIUM ALLOY WELDING WIRE 6A1 - 4V
SAE

SAE AMS3788/4A

In Force
1994-04-01
CLOTH, NYLON TWILL 5.5 Ounces per Square Yard (186 g/m2) Smooth Finish, Water Repellent Treated
SAE

SAE AMS4612L

In Force
2023-10-16
Brass, Naval, Bars and Rods, 60.5Cu - 38.5Zn - 0.75Sn, Hard Temper (H04)
SAE

SAE AMS4899E

In Force
2020-04-02
Titanium Alloy, Sheet, Strip, and Plate 4.5Al - 3V - 2Fe - 2Mo Annealed
SAE

SAE AMS4165E

In Force
1978-10-16
ALUMINUM ALLOY EXTRUSIONS 4.4Cu - 1.5Mg - 0.60Mn (2024-T3511) Stress-Relief Stretched and Straightened
SAE

SAE AMS4116D

In Force
1978-01-01
ALUMINUM ALLOY BARS, ROLLED, DRAWN, OR COLD FINISHED 1.0Mg - 0.60Si - 0.30Cu - 0.20Cr (6061-T4)
SAE

SAE AMS4778G

In Force
2000-09-01
Nickel Alloy, Brazing Filler Metal 92Ni - 4.5Si - 3.1B 1800 to 1900 °F Solidus-Liquidus Range
SAE

SAE AMS4730E

In Force
1994-04-01
NICKEL-COPPER ALLOY WIRE, CORROSION RESISTANT 67Ni - 31Cu Annealed (400)
SAE

SAE AMS4410A

In Force
2019-05-07
Aluminum Alloy Plate (7081-T7451) 7.2Zn - 1.5Cu - 2.0Mg - 0.10Zr Solution Heat Treated, Stress Relieved and Overaged
SAE

SAE AMS4615F

In Force
1995-04-01
Silicon Bronze Rods and Bars, 95.5cu 3.2si, Hard Temper
SAE

SAE AMS4447E

In Force
2000-10-01
Magnesium Alloy Castings, Sand 3.3Th - 2.1Zn - 0.75Zr (HZ32A-T5) Precipitation Heat Treated
SAE

SAE AMS4282D

In Force
1954-11-01
ALUMINUM ALLOY CASTINGS, PERMANENT MOLD 4.5Cu - 2.5Si (B195-T6) Solution and Precipitation Treated
SAE

SAE AMS4178C

In Force
1995-11-01
CORE, FLEXIBLE HONEYCOMB, ALUMINUM ALLOY, TREATED For Sandwich Construction 5052, 350 (177)
SAE

SAE AMS5524N

In Force
2025-07-25
Steel, Corrosion- and Heat-Resistant, Sheet, Strip and Plate 18Cr - 13Ni - 2.5Mo (SAE 316) Solution Heat Treated
SAE

SAE AMS4615E

In Force
1988-04-01
SILICON BRONZE RODS AND BARS, 95.5Cu - 3.2Si, Hard Temper
SAE

SAE AMS4900B

In Force
1963-01-15
TITANIUM SHEET, STRIP, AND PLATE Annealed, 55,000 psi Yield
SAE

SAE AMS4918K

In Force
2003-07-31
Titanium Alloy, Sheet, Strip, and Plate 6Al - 6V - 2Sn Annealed
SAE

SAE AMS4725A

In Force
1951-06-01
COPPER-BERYLLIUM ALLOY WIRE 98Cu - 1.9Be Solution Treated
SAE

SAE AMS4909D

In Force
1991-10-01
TITANIUM ALLOY SHEET, STRIP, AND PLATE 5Al - 2.5Sn, Extra Low Interstitial Annealed
SAE

SAE AMS4918B

In Force
1968-11-01
TITANIUM ALLOY SHEET, STRIP, AND PLATE 6A1 - 6V - 2Sn Annealed
SAE

SAE AMS4665A

In Force
1991-10-01
SILICON BRONZE TUBING, SEAMLESS 96Cu - 3.2Si Annealed
SAE

SAE AMS4363G

In Force
2006-06-21
Forgings, Magnesium Alloy, 2.0Th - 0.78Mn (HM21A - T5), Precipitation Heat Treated
SAE

SAE AMS4434H

In Force
1978-07-15
MAGNESIUM ALLOY CASTINGS, SAND 9.0Al - 2.0Zn (AZ92-T6)
SAE

SAE AMS5372B

In Force
1991-10-01
STEEL CASTINGS, SAND, CORROSION RESISTANT 16Cr - 1.9Ni (Type 431 Mod) Normalized and Tempered
SAE

SAE AMS4434G

In Force
1968-05-01
MAGNESIUM ALLOY CASTINGS, SAND 9Al - 2Zn (AZ92A-T6)
SAE

SAE AMS4223D

In Force
2012-09-26
Aluminum Alloy, Castings 4.5Cu - 0.70Ag - 0.30Mn - 0.25Mg - 0.25Ti (A201.0-T4) Solution Heat Treated and Naturally Aged
SAE

SAE AMS4434B

In Force
1944-08-01
MAGNESIUM ALLOY CASTINGS (Sand) 9 Al 2 Zn (Solution-Precipitation)
SAE

SAE AMS4409A

In Force
2021-05-18
Aluminum Alloy, Plate 4.0Zn - 2.0Mg - 0.32Mn (7019-T651) Solution Heat Treated, Stress Relieved, and Artificially Aged
SAE

SAE AMS3200F

In Force
1983-04-01
NITRILE RUBBER Petroleum-Base Hydraulic Fluid Resistant 55 - 65 (NBR Type)
SAE

SAE AMS2471J

In Force
2020-01-13
Anodic Treatment of Aluminum Alloys Sulfuric Acid Process, Undyed Coating
SAE

SAE AMS2424C

In Force
1991-10-01
NICKEL PLATING Low-Stressed Deposit
SAE

SAE AMS2375A

In Force
1978-04-15
CONTROL OF FORGINGS REQUIRING FIRST ARTICLE APPROVAL
SAE

SAE AMS3756B

In Force
2008-06-16
Moldings, Glass Fiber Filled Polytetrafluoroethylene (PTFE) 75% PTFE Resin, 25% Glass Fibers, As Sintered
SAE

SAE AMS4787B

In Force
1984-01-01
BRAZING FILLER METAL, HIGH TEMPERATURE 82Au - 18Ni 1740°F (950°C) Solidus-Liquidus Temperature
SAE

SAE AMS4239D

In Force
2006-09-22
Aluminum Alloy Castings, Sand, 6.8Mg - 0.18Ti - 0.18Mn (535.0-O), Annealed
SAE

SAE AMS4305

In Force
2017-09-21
Aluminum Alloy, Extruded Profiles (7449-T79511) 8.1Zn - 1.8Cu - 2.2Mg - 0.16Zr Solution Heat Treated, Stress Relieved, and Overaged
SAE

SAE AMS4900C

In Force
1968-11-01
TITANIUM SHEET, STRIP, AND PLATE Annealed, 55,000 psi Yield
SAE

SAE AMS4931E

In Force
2015-07-28
Titanium Alloy Bars, Forgings, and Rings 6Al - 4V Extra Low Interstitial (ELI) Duplex Annealed, Fracture Toughness
SAE

SAE AMS5070G

In Force
1994-04-01
STEEL BARS AND FORGINGS (0.18 - 0.23C) (SAE 1022)
SAE

SAE AMS4901E

In Force
1972-11-15
TITANIUM SHEET, STRIP, AND PLATE Annealed, 70,000 psi (483 MPa) Yield Strength
SAE

SAE AMS4366B

In Force
2026-04-21
Aluminum Alloy, Extruded Profiles (2065-T84), 4.2Cu - 1.2Li - 0.52Mg - 0.32Mn - 0.32Ag - 0.1Zr, Solution Heat Treated, Stress Relieved by Stretching and Artificially Aged
SAE

SAE AMS4782D

In Force
1994-07-01
NICKEL ALLOY, BRAZING FILLER METAL 71Ni - 10Si - 19Cr 1975 to 2075 °F (1080 to 1135 °C) Solidus-Liquidus Range
SAE

SAE AMS4619E

In Force
1977-01-01
Manganese Bronze Forgings, 58cu 39.8zn 1.05fe 0.95al 0.23mn
SAE

SAE AMS4418D

In Force
1979-10-15
MAGNESIUM ALLOY CASTINGS, SAND 2.5Ag - 2.1Di - 0.70Zr (QE22A-T6)
SAE

SAE AMS5070D

In Force
1973-05-01
STEEL BARS AND FORGINGS (0.18 - 0.23C) (SAE 1022)
SAE

SAE AMS4614G

In Force
1994-04-01
BRASS FORGINGS, FREE CUTTING 60Cu - 2.0Pb - 37.5Zn As Forged (M10)
SAE

SAE AMS4282A

In Force
1943-10-01
ALUMINUM ALLOY CASTINGS (Permanent Mold) 4 Copper - 2 Silicon (Solution Precipitation)
SAE

SAE AMS4779F

In Force
2000-09-01
Nickel Alloy, Brazing Filler Metal 94Ni - 3.5Si - 1.8B 1800 to 1950 °F (982 to 1066 °C) Solidus-Liquidus Range
SAE

SAE AMS4327

In Force
2009-06-10
Aluminum Alloy, Plate (2098-O) 3.5Cu - 1.1Li - 0.50Mg - 0.40Ag - 0.11Zr Annealed
SAE

SAE AMS4285D

In Force
2008-06-04
Aluminum Alloy Castings, Centrifugal 7.0Si - 0.30Mg (356.0-T6) Solution and Precipitation Heat Treated
SAE

SAE AMS4530A

In Force
1947-12-01
COPPER - BERYLLIUM ALLOY SHEET AND STRIP Solution Treated
SAE

SAE AMS4787E

In Force
1999-05-01
Gold-Nickel Alloy, Brazing Filler Metal, High Temperature 82Au - 18Ni 1740 °F (949 °C) Solidus-Liquidus Temperature
SAE

SAE AMS4223F

In Force
2025-08-01
Aluminum Alloy, Castings, 4.5Cu - 0.70Ag - 0.30Mn - 0.25Mg - 0.25Ti (A201.0-T4), Solution Heat Treated and Naturally Aged
SAE

SAE AMS5388D

In Force
1978-07-01
ALLOY CASTINGS, INVESTMENT, CORROSION AND HEAT RESISTANT 53.5Ni - 16.5Cr - 17Mo - 4.5W - 5.8Fe - 0.40V
SAE

SAE AMS4976N

In Force
2025-09-12
Titanium Alloy, Forgings, 6.0Al - 2.0Sn - 4.0Zr - 2.0Mo - 08Si, Solution and Precipitation Heat Treated
SAE

SAE AMS4083L

In Force
2012-11-27
Aluminum Alloy Tubing, Hydraulic, Seamless, Drawn, Round 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061-T6) Solution and Precipitation Heat Treated
SAE

SAE AMS4351B

In Force
2024-12-10
Aluminum Alloy, Plate (7065-T7651), 7.7Zn - 2.1Cu - 1.65Mg - 0.10Zr, Solution Heat Treated, Stress-Relieved, and Overaged