Filtrar:
SAE
SAE
SAE
SAE AMS5412A
In Force
2018-10-10
Steel Castings, Vacuum Melted, Vacuum Cast, Investment,
Corrosion-Resistant 13Cr - 8.0Ni - 2.2Mo - 1.1Al (195 ksi (1344 MPa)
Tensile Strength (Condition H1000) Homogenized, Solution, and
Precipitation Heat Treated
SAE
SAE AMS5611F
In Force
2013-08-12
Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Tubing, and
Rings 12Cr Ferrite Controlled, Consumable Electrode Melted
SAE
SAE AMS5568B
In Force
1981-07-01
STEEL TUBING, WELDED, CORROSION AND MODERATE HEAT RESISTANT 17Cr - 7.1Ni
- 1.1Al Solution Heat Treated, Precipitation-Hardenable
SAE
SAE AMS4772L
In Force
2023-01-17
Silver Alloy, Brazing Filler Metal 54Ag - 40Cu - 5.0Zn - 1.0Ni 1325 to
1575 °F (718 to 857 °C) Solidus-Liquidus Range
SAE
SAE AMS5558E
In Force
1996-08-01
STEEL, CORROSION AND HEAT RESISTANT, WELDED TUBING 18Cr - 10.5Ni -
0.70Cb (SAE 30347) Thin Wall Solution Heat Treated
SAE
SAE AMS4201E
In Force
2008-05-02
Aluminum Alloy Plate 6.2Zn - 2.3Cu - 2.2Mg - 0.12Zr (7050-T7651)
Solution Heat Treated, Stress Relieved, and Overaged
SAE
SAE AMS3894/8C
In Force
2016-11-10
Carbon Fiber Tape and Sheet Epoxy Resin Impregnated G 70000 (483)
Tensile, 36000000 (248) Modulus, 80 (176)
SAE
SAE AMS3826A
In Force
2011-08-09
CLOTH, TYPE "E" GLASS "B" Stage Polyester Resin
Impregnated 181 Type Fabric
SAE
SAE AMS5708L
In Force
2015-01-15
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Wire Forgings, and
Rings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B
Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C)
Solution Heat Treated
SAE
SAE AMS5719C
In Force
2000-03-01
Steel Bars, Wire, Forgings, Tubing, Rings, and Extrusions, Corrosion
Resistant 11.8Cr - 2.5Ni - 1.8Mo - 0.33V (0.08 - 0.15C) Annealed, Vacuum
Arc or Electroslag Remelted
SAE
SAE AMS4676F
In Force
2022-02-03
Nickel-Copper Alloy, Corrosion-Resistant, Bars and Forgings 66.5Ni -
3.0Al - 0.62Ti - 28Cu Hot-Finished, Precipitation Hardenable
SAE
SAE AMS5392J
In Force
1978-04-15
ALLOY IRON CASTINGS, SAND, MODERATE CORROSION AND HEAT RESISTANT 2.1Cr -
15Ni - 6.5Cu (2.4 - 2.8C)
SAE
SAE AMS5331E
In Force
1992-04-01
STEEL CASTINGS, SAND 0.82Cr - 1.8Ni - 0.35Mo (0.38 - 0.46C) (SAE 4340)
Normalized and Tempered
SAE
SAE
SAE
SAE AMS5400B
In Force
2007-12-13
Steel, Corrosion-Resistant, Investment Castings 15Cr - 4.6Ni - 0.22Cb -
2.8Cu Solution and Precipitation Heat Treated (H935) 170 ksi (1172 MPa)
Tensile Strength
SAE
SAE
SAE AMS5357B
In Force
2006-04-18
Steel, Corrosion Resistant, Investment Castings 15Cr - 4.6Ni - 0.22Cb -
2.8Cu Solution Heat Treated, Precipitation Hardenable
SAE
SAE AMS4046G
In Force
2017-06-15
Aluminum Alloy Sheet and Plate, Alclad One Side 5.6Zn - 2.5Mg - 1.6Cu -
0.23Cr (Alclad One Side 7075; -T6 Sheet -T651 Plate) Solution and
Precipitation Heat Treated
SAE
SAE AMS4168J
In Force
2008-05-02
Aluminum Alloy, Extrusions 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T6510)
Solution Heat Treated, Stress Relieved by Stretching, and Precipitation
Heat Treated, Unstraightened
SAE
SAE
SAE AMS5677A
In Force
1980-07-15
ALLOY WELDING ELECTRODES, COVERED, CORROSION AND HEAT RESISTANT 75Ni -
19.5Cr - 1.6 (Cb + Ta)
SAE
SAE
SAE AMS5558J
In Force
2021-12-13
Steel, Corrosion and Heat-Resistant, Welded Tubing 18Cr - 10.5Ni -
0.70Cb (Nb) (347) Thin Wall Solution Heat Treated
SAE
SAE AMS4125K
In Force
2009-08-05
Aluminum Alloy Die Forgings, and Rolled or Forged Rings 0.9Si – 0.62Mg –
0.25Cr (6151-T6) Solution and Precipitation Heat Treated
SAE
SAE AMS4221E
In Force
2016-12-13
Aluminum Alloy, Plate 4.4Cu - 1.5Mg - 0.60Mn (2124-T8151) Solution Heat
Treated, Stress Relieved, and Precipitation Heat Treated
SAE
SAE AMS4281B
In Force
1954-11-01
ALUMINUM ALLOY CASTINGS, PERMANENT MOLD 5Si - 1.2Cu - 0.5Mg (355-T6)
Solution and Precipitation Treated
SAE
SAE
SAE AMS5782D
In Force
2011-08-15
STEEL, CORROSION AND HEAT RESISTANT, WELDING WIRE 20.5Cr - 9.0Ni -
0.50Mo - 1.5W - 1.2(Cb+Ta) - 0.20Ti Vacuum Induction Melted
SAE
SAE AMS5751C
In Force
1981-04-01
ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 54Ni -
17.5Cr - 16.5Co - 4.0Mo - 2.9Ti - 2.9Al - 0.006B Solution,
Stabilization, and Precipitation Treated Consumable Electrode or Vacuum
Induction Melted
SAE
SAE AMS4983A
In Force
1994-11-01
TITANIUM ALLOY FORGINGS 10V - 2Fe - 3Al Consumable Electrode Melted,
Single Solution Heat Treated and Aged 180,000 psi (1240 MPa) Tensile Strength
SAE
SAE AMS4077G
In Force
2009-10-23
Aluminum Alloy Sheet and Plate, Alclad One Side 4.4Cu - 1.5Mg - 0.60Mn
(Clad One Side 2024-0) Annealed
SAE
SAE AMS4363E
In Force
1992-01-01
FORGINGS, MAGNESIUM ALLOY 2.0Th - 0.78Mn (HM21A - T5) Precipitation Heat Treated
SAE
SAE
SAE AMS4071E
In Force
1957-01-01
ALUMINUM ALLOY TUBING, HYDRAULIC, SEAMLESS, DRAWN 2.5Mg - 0.25Cr (5052-0)
SAE
SAE AMS5221A
In Force
1963-07-01
ALLOY STRIP Iron Base - 5.2Cr - 42Ni - 2.3Ti - 0.50Al Solution Treated
SAE
SAE
SAE AMS4972F
In Force
2007-10-16
Titanium Alloy Bars, Wire, and Rings 8Al - 1Mo - 1V Solution Heat
Treated and Stabilized
SAE
SAE
SAE AMS4385G
In Force
1984-10-01
MAGNESIUM ALLOY SHEET AND PLATE 3.2Th - 0.70Zr (HK31A-H24) Cold Rolled
and Partially Annealed
SAE
SAE
SAE AMS4177D
In Force
2011-11-03
Core, Flexible Honeycomb, Aluminum Alloy For Sandwich Construction 5056,
350 (177)
SAE
SAE AMS5641J
In Force
2021-10-12
Steel, Corrosion-Resistant, Bars, Wire, Forgings and Forging Stock
18.5Cr - 10Ni - 0.22Se (303Se) Free-Machining; for Swaging or Upsetting
Solution Heat Treated
SAE
SAE AMS4966N
In Force
2008-12-19
Titanium Alloy, Forgings 5Al - 2.5Sn Annealed, 110 ksi (758 MPa) Yield Strength
SAE
SAE AMS4323B
In Force
2008-05-02
Aluminum Alloy, Hand Forgings 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr
(7075-T7452) Solution Heat Treated, Stress Relieved, and Precipitation
Heat Treated
SAE
SAE AMS5336C
In Force
1982-04-01
STEEL CASTINGS, INVESTMENT 0.95Cr - 0.20Mo (0.25 - 0.35C) Normalized
SAE
SAE
SAE
SAE
SAE AMS4944G
In Force
2006-10-30
Titanium Alloy Tubing, Seamless, Hydraulic 3.0Al - 2.5V Cold Worked,
Stress Relieved
SAE
SAE AMS4301B
In Force
1991-04-01
BORON-ALUMINUM COMPOSITE SHEET 50 v/o 5.6B, 2024-0, For Diffusion Bonding
SAE
SAE AMS5666E
In Force
2000-03-01
Nickel Alloy, Corrosion and Heat Resistant, Bars, Forgings, Extrusions,
and Rings 62Ni - 21.5Cr - 9.0Mo - 3.65 (Cb+Ta) Annealed
SAE
SAE AMS4299
In Force
2012-04-03
Aluminum Alloy, Plate (7449-T7951) 8.1Zn - 1.8Cu - 2.3Mg Solution Heat
Treated, Stress Relieved, and Overaged
SAE
SAE AMS5380F
In Force
2007-09-13
Cobalt Alloy, Corrosion and Heat Resistant, Investment Castings 50.5Co -
26Cr - 15Ni - 6.0Mo As Cast
SAE
SAE AMS5642G
In Force
1976-07-01
STEEL BARS AND FORGINGS, CORROSION AND HEAT RESISTANT 18Cr - 10.5Ni -
0.60 (Cb + Ta) (303 + Cb) Free-Machining
SAE
SAE
SAE AMS4027E
In Force
1964-06-01
ALUMINUM ALLOY SHEET AND PLATE 1.0Mg - 0.60Si - 0.25Cu - 0.25Cr (6061-T6)
SAE
SAE AMS5501E
In Force
2013-08-12
Steel, Corrosion Resistant, Sheet, Strip, and Foil 19Cr - 9.5Ni (304)
Cold Rolled, 125 ksi (862 MPa) Tensile Strength